Rutile-coated rod electrode
EutecTrode E310-17
Rutile coated stick electrode with approx. 120 % yield. Fully austenitic, corrosion-resistant weld metal. Scale resistant up to 1150 °C (air). Maximum operating temperature of 300 °C for dissimilar joints.
Technical data
EN ISO 3581-A: E 25 20 R 32
AWS A5.4: E310-17
SFA 5.4: E310-17
Material no.: 1.4842
Applications
For joint welding of alloy-like, heat-resistant CrNi steels, e.g:
1.4837 - GX 40 CrNiSi 25-12,
1.4840 - GX 15 CrNi 25-20,
1.4841 - X 15 CrNiSi 25-20,
1.4843 - X 12 CrNi 25-20,
1.4845 - X 12 CrNi 25-21,
for welding ferritic Cr steels and for mixed joints of austenitic stainless steels, e.g:
1.4301 - X 5 CrNi 18-10 (X 5 CrNi 18-9),
1.4306 - X 2 CrNi 19-11 (X 2 CrNi 18-9),
1.4308 - GX 6 CrNi 18-9,
1.4401 - X 5 CrNiMo 17-12-2 (X 5 CrNiMo 18-10),
1.4404 - X 2 CrNiMo 17-13-2 (X 2 CrNiMo 18-10),
1.4408 - GX 6 CrNiMo 18-10,
1.4435 - X 2 CrNiMo 18-14-3 (X 2 CrNiMo 18-12),
1.4436 - X 5 CrNiMo 17-13-3 (X 5 CrNiMo 18-12),
1.4541 - X 6 CrNiTi 18-10,
1.4550 - X 6 CrNiNb 18-10 (X 10 CrNiNb 18-9),
1.4552 - GX 5 CrNiNb 18-9,
1.4571 - X 6 CrNiMoTi 17-12-2,
1.4573 - X 10 CrNiMoTi 18-12,
1.4580 - X 6 CrNiMoNb 17-12-2,
1.4581 - GX 5 CrNiMoNb 18-10,
1.4583 - X 10 CrNiMoNb 18-12,
1.4948 - X 6 CrNi 18-11
with unalloyed and low-alloy steels, e.g:
P 235 GH, P 265 GH, P 295 GH, 16 Mo 3, S 255 N to P 355 N, cast steel and manganese steels; also for build-up welding.
Processing instructions
Clean welding areas. Re-dry at 250 °C / 3 h. Limit interpass temperature to 100 °C. Use stick bead technique with low line energy. Use wire brushes made of austenitic CrNi steels.
Welding positions: all, except PG (f)
Type of current: = (+) or ~
Open circuit voltage: ≥ 70 V
Specification
Code | 102212 |
---|---|
Category | Highly alloyed |
Number in package | 5.0 Kg |
Price per unit | 485,718 kr / Kg |
Price excl. VAT | 2.428,59 kr |
Price incl. VAT 25% | 3.035,74 kr |
Availability | within 7 to 10 days |