Rutile-coated rod electrode
EutecTrode E309L-17
Rutile coated stick electrode with approx. 115 % yield. Austenitic weld metal with approx. 15 % δ-ferrite. Resistant to intergranular corrosion up to 400 °C. Scale resistant up to 1050 °C. The lowest permissible operating temperature is -60 °C. Maximum permissible operating temperature of 350 °C.
Technical data
EN ISO 3581-A: E 23 12 L R 32
AWS A5.4: E309L-17
SFA 5.4: E309L-17
Material no.: 1.4332
Ferrite: 15 FN
Applications
For mixed joints of stainless, austenitic steels, e.g:
1.4301 - X 5 CrNi 18-10 (X 5 CrNi 18-9),
1.4306 - X 2 CrNi 19-11 (X 2 CrNi 18-9),
1.4308 - GX 6 CrNi 18-9,
1.4311 - X 2 CrNiN 18-10,
1.4401 - X 5 CrNiMo 17-12-2 (X 5 CrNiMo 18-10),
1.4404 - X 2 CrNiMo 17-13-2 (X 2 CrNiMo 18-10),
1.4408 - GX 6 CrNiMo 18-10,
1.4435 - X 2 CrNiMo 18-14-3 (X 2 CrNiMo 18-12),
1.4436 - X 5 CrNiMo 17-13-3 (X 5 CrNiMo 18-12),
1.4541 - X 6 CrNiTi 18-10,
1.4550 - X 6 CrNiNb 18-10 (X 10 CrNiNb 18-9),
1.4552 - GX 5 CrNiNb 18-9,
1.4571 - X 6 CrNiMoTi 17-12-2,
1.4573 - X 10 CrNiMoTi 18-12,
1.4580 - X 6 CrNiMoNb 17-12-2,
1.4581 - GX 5 CrNiMoNb 18-10,
1.4583 - X 10 CrNiMoNb 18-12,
1.4948 - X 6 CrNi 18-11
with unalloyed and low-alloy steels, e.g:
P 235 GH, P 265 GH, P 295 GH, 16 Mo 3, S 255 N to P 355 N
and corresponding cast steel, also for corrosion-resistant weld cladding on the above-mentioned unalloyed and low-alloy steels and on heat-resistant, tempered fine-grain structural steels in accordance with AD 2000-Merkblatt HP 0, Group 3.
Processing instructions
Clean welding areas. Re-dry at 250 °C /3 h. Limit interpass temperature to 150 °C. Use wire brushes made of austenitic CrNi steels.
Welding positions: all, except PG (f)
Type of current: = (+) or ~
Open circuit voltage: ≥ 50 V
Approvals
TÜV, CE
Specification
Code | 102206 |
---|---|
Category | Highly alloyed |
Number in package | 5.0 Kg |
Price per unit | 50,97 € / Kg |
Price excl. VAT | 254,85 € |
Price incl. VAT 25.5% | 319,84 € |