EnDOtec DO*519 S Flux-cored wire

Flux-cored wire for cladding and dissimilar metal joints

EnDOtec DO*519 S, Ø 1.2 mm, 15.0 kg

Rutile-basic flux-cored wire designed for fabrication, joints and overlays where high reliability and dependability are required.
Recommended for joining and fabricating where dissimilar steels are welded (dissimilar joints), such as CrNi steels with non-low-alloy steels.
Fully austenitic weld metal with approx. 20 % δ-ferrite.
Excellent resistance to intergranular corrosion and pitting. Admissible operating temperatures between -120°C and +400°C. For dissimilar joints, the maximum operating temperature is 300°C.

  • High arc stability.
  • Low heat input, low dilution.
  • Excellent weldability in all positions.
  • Easy slag removal.
  • High deposition rate.

Technical data
EN ISO 17633-A: T 23 12 2 L P C/M 1
AWS A5.22: E309LMo T1-1/4
W.-Nr.: 1.4459

Applications
Industry and equipment in general, in particular:
Chemical and pharmaceutical. Petrochemical plants, refineries. Food industry: sugar factories, dairy industry, wine industry. Breweries and all types of boiler construction. Containers, heat exchangers.

Processing instructions

  • Welding equipment
    The flux cored wire DO*519 S is fully compatible with conventional power sources. Programmable units with pulsed arcs provide optimum performance.

  • Preparation
    Before welding, the workpiece must be provided with a bevel for X or V welds, which is particularly suitable for thick welds. The areas to be welded and the surrounding area must be kept particularly clean.

  • Preheating
    Preheating is not normally necessary for stainless steels. However, if ferritic steel is to be joined to austenitic steel, it may be necessary to preheat the ferritic area, depending on the type and size of the workpiece to be welded.

  • Welding parameters
    Welding current and polarity: DC= (+)
    Stick-out: 15 – 20 mm
    Ø (mm) 1.2 
    Voltage (V) 20 – 34 
    Current (A) 120 – 280

  • Welding technique
    To achieve a better penetration for welds where several passes are required, the welding torch must be held at an angle of 70 – 80°.

  • Machining the weld
    The weld metal can be machined or ground and can be cut with a gouging torch (Arc-Air) or a plasma arc.

  • Shielding gas
    Recommended gas: 82% Ar, 18% CO2 [ISO 14175 M21]
    Alternative gas: 98% Ar, 2% CO2 [ISO 14175 M12]
    Flow (l/min): 14

  • Welding positions
    PA, PB, PC, PD, PE, PF, PG [ISO 06947]

Approvals
TÜV, DB

Specification

Code 764006
Category Highly alloyed
Number in package 15.0 kg
Price per unit 260,6993 kr / kg
Price excl. VAT 3.910,49 kr
Price incl. VAT 25% 4.888,11 kr
Availability within 7 to 10 days
Material Safety data Sheets

Other products in the category