CastoWig 45252 W TIG welding rod Ø 3.0mm

for high-temperature CrMo steels

CastoWig 45252W

CrMo-alloyed weld metal with high high-temperature strength up to 570 °C. The lowest operating temperature is -10 °C. Hardness increase through case hardening, nitriding or tempering.

Technical data
DIN EN ISO 21952 A: W CrMo1Si
Material no.: 1.7339
AWS A5.28: ER80S-G

Applications
For joint welding of heat-resistant, CrMo-alloyed boiler and pipe steels, e.g:
1.7335 - 13 CrMo 4 5
1.7357 - GS-17 CrMo 5 5
and corresponding cast and pipe materials, as well as similar low-alloy case-hardening and heat-treatable steels.
quenched and tempered steels.
Typical application examples are
Components from steam boiler, pressure vessel and pipeline construction.

Processing instructions
Clean welding areas. Adjust the heat input during welding to the component, its material and dimensions, preheat alloy-like steels to 200 - 250 °C. Ensure a continuous
filler material supply.
After welding, a tempering treatment (680 °C / 2 h / air cooling) is required.

Welding positions: all, except PG (f)
Type of current: = (-)
Shielding gas: EN ISO 14175 - I1 (100 % Ar)

Approval
TÜV, DB (42.024.09), CE

Specification

Code 330312
Category Unalloyed and low-alloyed
Number in package 5.0 kg
Price per unit 31,194 £ / kg
Price excl. VAT 155,97 £
Price incl. VAT 20% 187,16 £
Availability within 5 to 10 days
Diameter:
Material Safety data Sheets